    "help": "Return the metadata of a dataset (package) and its resources. :param id: the id or name of the dataset :type id: string",
    "success": true,
    "result": {
        "id": "43775bda-6c4c-4060-8ff8-c847d2a6094e",
        "url": "https://www.inptdat.de/node/101",
        "source": {
            "name": "HelixJet, HF plasma jet, CCP",
            "application": "additive manufacturing, film deposition, PECVD",
            "specification": "AC, high frequency, atmospheric pressure, non-thermal",
            "properties": "<p>Non-thermal atmospheric pressure plasma jet (capacitively coupled). Power: 50 W; Frequency: 27.12 MHz; Flow rate: 1000\u2009sccm Ar; Electrodes: helical configuration with inclination angle 33\u00b0; Capillary: inner diameter 7 mm.</p>\n",
            "procedure": "<p>The measurements occur 30 minutes after temperature conditioning of the plasma source.</p>\n"
        },
        "medium": {
            "name": "Ar",
            "properties": "<p>Flowrate: 1000\u2009sccm; Pressure: 1 bar; Temperature: 300 to 1000 K; Purity: argon 6.0</p>\n",
            "procedure": "<p>Standard conditions of the argon gas are assured.</p>\n"
        },
        "target": {
            "name": "Polyamide 12",
            "properties": "Polyamide 12 powder with mean diameter of 60 \u00b5m at room temperature.",
            "procedure": "Dosis: 10\u2009mg in 50\u2009ms introduced in the argon flow. Footprint area: 1\u2009cm\u00b2 at 1 cm below the outlet of the jet. "
        },
        "diagnostics": {
            "name": "thermographic imaging, fast imaging",
            "properties": "<p>The process has been captured with a high-speed infrared camera Flir SC6801 F/2.5 3-5 \u00b5m combined with infrared microscope objective \u00d71 at the frame rate of 2 kHz (320\u00d7256 pixel). The optic system with InSb detector (640\u00d7512 pixel) is calibrated for temperatures from -10\u00b0C to 350\u00b0C. The working distance was 6.1 mm from the axis of the HelixJet.</p>\n"
        },
        "resource": [
            {
                "id": "73f9ee9b-9b98-4b88-8d9a-9d095a09cd90",
                "url": "https://www.inptdat.de/system/files/node101_movie.mp4",
                "filetype": "mp4",
                "datatype": "high-speed video",
                "range": "Feeding of 10\u2009mg/50\u2009ms  Polyamide 12 powder with mean diameter of 60 \u00b5m into argon plasma with flow rate of 1000\u2009sccm at a power of 50 W.",
                "quality": "verified"
            }
        ]
    }
}